Description
General use for tin, lead alloys, zinc alloys, polyester, and polyurethane used in spin casting. Long mold life, with high temperature resistance.
Phone
+1 239 3713848$36.00
VULCANIZATION TEMP. 175 °C
VULCANIZATION TIME 45 min/7 mm of mould thickness
HARDNESS 68 Shore A
General use for tin, lead alloys, zinc alloys, polyester, and polyurethane used in spin casting. Long mold life, with high temperature resistance.